Site occupation evolution of alloying elements in L12 phase during phase transformation in Ni75Al7.5
Correlation between site occupation evolution of alloying elements in L12 phase and growth of DO22 phase in Ni75Al7.5V17......
采用双真空熔炼法,通过部分置换W制备含Co和不含Co的镍基高温合金。系统研究合金在900℃下的氧化与75%Na2SO4+25%NaCl(质量分数)熔......